Manganese is a strategic element playing a vital role in various industries, including steelmaking, batteries, pigments, and pharmaceuticals. Although the majority of produced manganese is consumed in the steel industry, its non-metallurgical applications, particularly in the production of high-purity manganese dioxide nanoparticles, have gained increasing importance. Achieving the quality required for these applications necessitates the use of high-purity manganese solutions with minimal impurities. To this end, the recovery of manganese from low-grade ores remains a significant challenge due to the presence of carbonate and silicate impurities. In this study, a two-stage gravity separation-acid leaching process was developed for the beneficiation of low-grade manganese ore (13.8% MnO). In the first stage, the use of a shaking table significantly reduced gangue minerals, resulting in a concentrate containing 38.9% MnO. In the second stage, acid leaching with hydrochloric and sulfuric acids was performed to remove the remaining carbonate phases. Parameters affecting the leaching process—including acid type and concentration, temperature, and reaction time—were systematically investigated, and the resulting products were evaluated using XRF, XRD, and SEM-EDX analyses. The results demonstrated that under optimal conditions, over 97% of calcium was removed, and a final product with 69.71% MnO (pyrolusite purity exceeding 85%) was obtained. This product, containing quartz and barite as the primary insoluble impurities in reductive manganese leaching, can be utilized as a potential precursor for the synthesis of manganese oxide compounds. Overall, this approach paves the way for the production of high-quality manganese concentrate for advanced industrial and nanotechnology applications.
کلیدواژهها English