Amirkabir Journal of Civil Engineering

Amirkabir Journal of Civil Engineering

Experimental design and modeling of sulfur removal parameters from magnetic iron concentrates by reverse flotation method

Document Type : Research Article

Authors
1 Master of Mineral Processing, Lorestan University
2 mining grope-lorestan university
Abstract
Sarab Mining Complex is one of the producers of iron concentrate in Kurdistan Province . The d80 of magnetic separation concentrate products had dimensions of about 38.42 microns and the average sulfur and iron grades were about 7.2 and about 63.24, respectively. XRD results showed that this concentrate consists of magnetite, pyrrhotite, pyrite, grossular, serpentine and dolomite minerals. The presence of sulfur in the form of pyrrhotite and pyrite minerals reduces the flexibility and strength of steel and causes brittleness of steel, so the reverse flotation method was used to remove sulfur in the concentrate, and parameters such as collector, foaming agent, pulp solids percentage, activator and pH were investigated using the experimental design method. The results obtained under optimal conditions show that under conditions of potassium amyl xanthate amount of 1315 g/ton, pH of about 4.5, foaming agent amount of about 126 g/ton, pulp solids percentage of 35 percent and activator amount of 210 g/ton, the sulfur content is reduced from 7.2 to 4.1 percent. Before the flotation operation, by activating the pyrrhotite surfaces with oxalic acid at a concentration of 0.0004 mol/liter in water for one hour, the sulfur content of the magnetic concentrate can be increased from 7.2% to 1.2% by reverse flotation (under optimal conditions), and about 83.33% of the sulfur in the magnetic concentrate can be removed. by preparing the magnetic concentrate sample with oxalic acid, the sulfur removal percentage in the magnetic concentrate can be improved by 2.9%.
Keywords